Spoolarac 80 is a low manganese and silicon wire. It provides excellent ductility and crack resistance. Typical applications include lap welds, build-up, or repair welding prior to machining.
Low manganese and silicon wire - minimal rust and mill scale tolerance. Excellent ductility and crack resistance - recommended for restrained welds and good machinability. Suitable for butt or fillet welds on lower strength carbon steels. Applications include high speed lap welds, build-up or repair welding prior to machining and buttering or cladding operations.

| C | 0.09 % |
|---|---|
| Mn | 0.4 % |
| Si | 0.04 % |
| P | 0.005 % |
| S | 0.010 % |
| Typical wire analysis | |
| C | 0.10 % |
| Mn | 0.44 % |
| Si | 0.04 % |
| P | 0.003 % |
| S | 0.014 % |
| Diameter | Wire Feed Speed | Amps | Volts | Deposition Rate |
|---|---|---|---|---|
| .023 in, 0.6 mm | 400 ipm, 1016 cm/min | 100 | 23 | 2.7 lbs./hr., 1.2 kg./hr. |
| 450 ipm, 1143 cm/min | 106 | 23 | 3.1 lbs./hr., 1.4 kg./hr. | |
| 500 ipm, 1270 cm/min | 111 | 24 | 3.4 lbs./hr., 1.6 kg./hr. | |
| 550 ipm, 1397 cm/min | 117 | 24 | 3.8 lbs./hr., 1.7 kg./hr. | |
| 600 ipm, 1524 cm/min | 122 | 25 | 4.1 lbs./hr., 1.9 kg./hr. | |
| 630 ipm, 1600 cm/min | 125 | 25 | 4.3 lbs./hr., 2 kg./hr. | |
| .030 in, 0.8 mm | 500 ipm, 1270 cm/min | 160 | 24 | 5.8 lbs./hr., 2.6 kg./hr. |
| 550 ipm, 1397 cm/min | 173 | 25 | 6.4 lbs./hr., 2.9 kg./hr. | |
| 600 ipm, 1524 cm/min | 187 | 25 | 7 lbs./hr., 3.2 kg./hr. | |
| 650 ipm, 1651 cm/min | 200 | 26 | 7.6 lbs./hr., 3.4 kg./hr. | |
| .035 in, 0.9 mm | 400 ipm, 1016 cm/min | 180 | 25 | 6.3 lbs./hr., 2.9 kg./hr. |
| 450 ipm, 1143 cm/min | 197 | 26 | 7.1 lbs./hr., 3.2 kg./hr. | |
| 500 ipm, 1270 cm/min | 213 | 26 | 7.9 lbs./hr., 3.6 kg./hr. | |
| 550 ipm, 1397 cm/min | 230 | 27 | 8.7 lbs./hr., 4 kg./hr. | |
| .045 in, 1.2 mm | 300 ipm, 762 cm/min | 260 | 25 | 7.9 lbs./hr., 3.6 kg./hr. |
| 350 ipm, 889 cm/min | 280 | 26 | 9.2 lbs./hr., 4.2 kg./hr. | |
| 400 ipm, 1016 cm/min | 300 | 28 | 10.5 lbs./hr., 4.8 kg./hr. | |
| 450 ipm, 1143 cm/min | 320 | 29 | 11.8 lbs./hr., 5.4 kg./hr. | |
| 500 ipm, 1270 cm/min | 340 | 30 | 13.1 lbs./hr., 6 kg./hr. | |
| .052 in, 1.3 mm | 265 ipm, 673 cm/min | 275 | 26 | 9.3 lbs./hr., 4.2 kg./hr. |
| 300 ipm, 762 cm/min | 310 | 28 | 10.5 lbs./hr., 4.8 kg./hr. | |
| 350 ipm, 889 cm/min | 360 | 31 | 12.2 lbs./hr., 5.6 kg./hr. | |
| 390 ipm, 991 cm/min | 400 | 33 | 13.6 lbs./hr., 6.2 kg./hr. | |
| .062 in, 1.6 mm | 180 ipm, 457 cm/min | 290 | 26 | 9.1 lbs./hr., 4.1 kg./hr. |
| 200 ipm, 508 cm/min | 310 | 28 | 10.1 lbs./hr., 4.6 kg./hr. | |
| 230 ipm, 584 cm/min | 340 | 31 | 11.6 lbs./hr., 5.3 kg./hr. | |
| 260 ipm, 660 cm/min | 370 | 34 | 13.2 lbs./hr., 6 kg./hr. | |
| 280 ipm, 711 cm/min | 390 | 36 | 14.2 lbs./hr., 6.4 kg./hr. |