Print this page

Spoolarc 81

Spoolarc 81 is a medium manganese and silicon wire with nominal rust and mill scale tolerance. Typical applications include structural steels, medium strength pressure vessels, ship, barge, and offshore oil rig fabrication.

Features

Medium manganese and silicon wire - nominal rust and mill scale tolerance.
Developed for general purpose welding on low and medium carbon steels.
Applications include structural steels, medium strength pressure vessels, ship, barge and offshore oil rig fabrication.
Use with OK Flux 50, 80, 429, 231, 350, 10.71, 10.72, and 10.62 fluxes.

Spoolarc 81
  • Welding Process
  • SAW (Sub Arc)

Classifications

  • Classifications/Approvals

    • AWS/ASME SFA 5.17; EM12K
    • ABS/AWS A5.17; EM12K
    • Certified by CWB to CSA W48

Properties

Typical Properties
C 0.1 %
Mn 1.0 %
Si 0.2 %
P 0.008 %
S 0.010 %
Typical wire analysis  
C 0.11 %
Mn 0.95 %
Si 0.26 %
P 0.006 %
S 0.008 %

SAW

Accessories

Depositions

Spray Transfer Deposition Table
Diameter Amps Deposition Rate Average Deposition Efficiency
1/16 in, 1.6 mm 400 13.0 lbs./hr., 5.90 kg./hr. 99 %
500 17.0 lbs./hr., 7.71 kg./hr. 99 %
5/64 in, 2.0 mm 300 10.8 lbs./hr., 4.90 kg./hr. 99 %
400 14.5 lbs./hr., 6.58 kg./hr. 99 %
500 18.2 lbs./hr., 8.26 kg./hr. 99 %
3/32 in, 2.4 mm 400 13.2 lbs./hr., 5.99 kg./hr. 99 %
500 17.0 lbs./hr., 7.71 kg./hr. 99 %
600 22.0 lbs./hr., 9.98 kg./hr. 99 %
1/8 in, 3.2 mm 400 11.0 lbs./hr., 4.99 kg./hr. 99 %
500 14.5 lbs./hr., 6.58 kg./hr. 99 %
600 18.0 lbs./hr., 8.16 kg./hr. 99 %
700 21.2 lbs./hr., 9.62 kg./hr. 99 %
5/32 in, 4.0 mm 500 12.5 lbs./hr., 5.67 kg./hr. 99 %
600 16.0 lbs./hr., 7.26 kg./hr. 99 %
700 19.5 lbs./hr., 8.85 kg./hr. 99 %
800 23.0 lbs./hr., 10.43 kg./hr. 99 %
900 26.0 lbs./hr., 11.79 kg./hr. 99 %
3/16 in, 4.8 mm 600 13.9 lbs./hr., 6.31 kg./hr. 99 %
700 17.5 lbs./hr., 7.94 kg./hr. 99 %
800 21.0 lbs./hr., 9.53 kg./hr. 99 %
900 25.0 lbs./hr., 11.34 kg./hr. 99 %
1000 29.2 lbs./hr., 13.25 kg./hr. 99 %
1100 34.0 lbs./hr., 15.42 kg./hr. 99 %

Extra Info