SPOOLARC 100

Spoolarc 100 is a Cr, Ni, Mo alloyed submerged arc welding wire suitable for welding of high strength, low alloy quenched and tempered steels.

Features

Designed for low alloy quenched and tempered steels. Weld metal mechanical properties include high yield strength (exceeds 100 ksi/690 MPa) and low temperature impact toughness. Applications include heat treatable valves and fittings, structural weldments and low temperature pipe valves.

SPOOLARC 100
  • Welding Process
  • SAW (Sub Arc)

Classifications

  • Classifications/Approvals

    • AWS/ASME SFA5.23 EF5

Properties

Typical Properties
Typical Wire Analysis  
C 0.12 %
Mn 1.9 %
Si 0.1 %
P 0.006 %
S 0.006 %
Cr 0.4 %
Ni 2.4 %
Mo 0.5 %
Cu 0.3 %
Wire Chemistries  
C 0.12 %
Mn 1.91 %
Si 0.07 %
P 0.007 %
S 0.006 %
Cr 0.38 %
Ni 2.40 %
Mo 0.50 %
Other Cu 0.32  

SAW

Accessories

Depositions

Spray Transfer Deposition Table
Diameter Wire Feed Speed Amps Volts Deposition Rate
.023 in, 0.6 mm 400 ipm, 1016 cm/min 100 23 2.7 lbs./hr., 1.2 kg./hr.
450 ipm, 1143 cm/min 106 23 3.1 lbs./hr., 1.4 kg./hr.
500 ipm, 1270 cm/min 111 24 3.4 lbs./hr., 1.5 kg./hr.
550 ipm, 1397 cm/min 117 24 3.8 lbs./hr., 1.7 kg./hr.
600 ipm, 1524 cm/min 122 25 4.1 lbs./hr., 1.8 kg./hr.
630 ipm, 1600 cm/min 125 25 4.3 lbs./hr., 1.9 kg./hr.
.030 in, 0.8 mm 500 ipm, 1270 cm/min 160 25 5.8 lbs./hr., 2 kg./hr.
550 ipm, 1397 cm/min 173 25 6.4 lbs./hr., 2.9 kg./hr.
600 ipm, 1524 cm/min 187 25 7 lbs./hr., 3.1 kg./hr.
650 ipm, 1651 cm/min 200 26 7.6 lbs./hr., 3.4 kg./hr.
.035 in, 0.9 mm 400 ipm, 1016 cm/min 180 26 6.3 lbs./hr., 3.4 kg./hr.
450 ipm, 1143 cm/min 197 26 7.1 lbs./hr., 3.2 kg./hr.
500 ipm, 1270 cm/min 213 26 7.9 lbs./hr., 3.5 kg./hr.
550 ipm, 1397 cm/min 230 27 8.7 lbs./hr., 3.9 kg./hr.
.045 in, 1.2 mm 300 ipm, 762 cm/min 260 27 7.9 lbs./hr., 4 kg./hr.
350 ipm, 889 cm/min 280 26 9.2 lbs./hr., 4.1 kg./hr.
400 ipm, 1016 cm/min 300 27 10.5 lbs./hr., 4.6 kg./hr.
450 ipm, 1143 cm/min 320 29 11.8 lbs./hr., 5.2 kg./hr.
500 ipm, 1270 cm/min 340 30 13.1 lbs./hr., 5.8 kg./hr.
.052 in, 1.3 mm 265 ipm, 673 cm/min 275 30 9.3 lbs./hr., 6 kg./hr.
300 ipm, 762 cm/min 310 27 10.5 lbs./hr., 4.6 kg./hr.
350 ipm, 889 cm/min 360 30 12.2 lbs./hr., 5.4 kg./hr.
390 ipm, 991 cm/min 400 32 13.6 lbs./hr., 6 kg./hr.
.062 in, 1.6 mm 180 ipm, 457 cm/min 290 33 9.1 lbs./hr., 6.2 kg./hr.
200 ipm, 508 cm/min 310 27 10.1 lbs./hr., 4.4 kg./hr.
230 ipm, 584 cm/min 340 30 11.6 lbs./hr., 5.1 kg./hr.
260 ipm, 660 cm/min 370 33 13.2 lbs./hr., 5.8 kg./hr.
280 ipm, 711 cm/min 390 35 14.2 lbs./hr., 6.2 kg./hr.