Spoolarc U515 is a submerged arc wire that is used for welding Cr-Mo steels up to 1-1/4% Cr and 1/2% Mo. Typical applications include process piping, heat exchangers, and pressure vessel fabrication.
Designed for use on low alloy steels up to 1.25% Cr - 0.5% Mo. Applications include process piping, heat exchangers and pressure vessel fabrication.

| C | 0.13 % |
|---|---|
| Mn | 0.7 % |
| Si | 0.15 % |
| P | 0.006 % |
| S | 0.011 % |
| Cr | 1.6 % |
| Mo | 0.5 % |
| Typical wire analysis | |
| C | 0.10 % |
| Mn | 0.65 % |
| Si | 0.18 % |
| P | 0.010 % |
| S | 0.010 % |
| Cr | 1.50 % |
| Mo | 0.50 % |