Print this page

SPOOLARC WS

Spoolarc WS is an ER80S-G special purpose wire designed to weld "weathering" grade steels.

Features

Spoolarc WS is a special purpose wire designed to weld "weathering" grade steels. The weld metal properties provide the color matching characteristics desired for ASTM A588, A242, Cor-Ten and Mayari R® steels. The mechanical properties meet the Federal Highway (AASHTO) Charpy impact standards of 25 ft.-lbs. (34 J) @ -20ºF (-29ºC). Applications for Spoolarc WS include butt and fillet welds on structural support members and other fabrication requirements for welding weathering grade steels.

Classifications

  • Classifications/Approvals

    • AWS/ASME SFA 5.23 ER80S-3
    • AWS/ASME SFA 5.28 ER80S-3

Properties

Typical Properties
As Welded GMAW 98% Ar / 2% O2  
Yield Strength 72 ksi, 500 MPa
Tensile Strength 78 ksi, 540 MPa
Elongation in 2" 24 %
Typical Charpy V-Notch Impact Properties  
Testing Temperature -20°F (-29°C)  
As Welded GMAW 98% Ar / 2% O2 25 ft.-lbs., 34 J
Typical Undiluted Weld Metal Analysis  
GMAW 98% Ar / 2% O2  
C 0.1 %
Mn 0.55 %
Si 0.23 %
P 0.014 %
S 0.009 %
Cr 0.45 %
Ni 0.55 %
Cu 0.45 %
Typical Wire Analysis  
C 0.08 %
Mn 0.5 %
Si 0.2 %
P 0.004 %
S 0.008 %
Cr 0.6 %
Ni 0.5 %
Cu 0.5 %

SAW

Accessories

Depositions

Extra Info