Sureweld SW-14 is an all-position electrode designed for use with AC. It produces an easily controlled, forceful arc with deep penetration and a high quality weld metal.

Features

Sureweld SW-14 is an all-position cellulosic electrode designed for AC. It produces an easily controlled forceful arc with deep penetration and a high quality weld metal which will pass specification requirements for radiography. SW-14 is used primarily for welding mild steels such as ASTM A-36, A-283, A-284, A-285, A-515, A-516 and ABS Hull and Boiler Steel. Typical applications include welding of buildings, piping, shipbuilding, pressure vessels and tanks.

AC-DCEP (Electrode Positive)

SUREWELD SW-14
  • Industry
  • General Fabrication
  • Welding Process
  • SMAW (Stick)

Classifications

  • Classifications/Approvals

    • ASME SFA 5.1
    • AWS A5.1; E6011
    • A.B.S.- AWS A5.1; E6011
    • CERTIFIED BY C.W.B.- CSA W48

Properties

Typical Properties
As Welded  
Yield Strength 66 ksi, 460 MPa
Tensile Strength 76 ksi, 525 MPa
Reduction in Area 56
Elongation in 2" 22 %
Typical Charpy V-Notch Impact Properties  
Testing Temperature -20ºF (-29ºC)  
As Welded 31 ft.-lbs., 42 J
Typical Undiluted Weld Metal Analysis  
C 0.1 %
Mn 0.36 %
Si 0.15 %
P 0.012 %
S 0.016 %

SAW

Accessories

Depositions

Deposition Table
Diameter Optimal Amperage Range Amperage Deposition Rate Efficiency
3/32 in, 2.4 mm 75 A 60 - 80 1.3 lbs./hr., 0.6 kg./hr. 61 %
1/8 in, 3.2 mm 100 A 90 - 130 2.3 lbs./hr., 1 kg./hr. 70.7 %
5/32 in, 4.0 mm 140 A 130 - 160 3.7 lbs./hr., 1.7 kg./hr. 77 %
3/16 in, 4.8 mm 160 A 155 - 190 4.1 lbs./hr., 1.9 kg./hr. 73.4 %
7/32 in, 5.6 mm 190 A 175 - 220 5 lbs./hr., 2.3 kg./hr. 74.2 %
1/4 in, 6.4 mm 250 A 225 - 260 5.6 lbs./hr., 2.5 kg./hr. 71.9 %

Extra Info

Procedure

  • Hold a medium to short arc tilted 5° to 15° in the direction of travel with the electrode at an angle of 45° to each plate in fillet welds. Weave with slight oscillating motion, hesitating at the edges to insure proper fusion. Clean slag before depositing next bead.