SUREWELD SW-15

Sureweld SW-15 is an all-position electrode that can be used for a wide range of applications for light gauge and heavyplate. High heat and speeds can be used without undercut. The slag is easy to clean and even self-cleaning on heavy plate.

Features

Sureweld SW-15 is a versatile electrode with a wide range of applications for light gauge and heavy plate. High heat and speeds can be used without undercut. Slag is easy to clean and on heavy plates is often self-cleaning.
SW-15 can be used in many applications. Typical applications include metal fixtures, road equipment, farm machinery, building structures, storage tanks and ironwork.

Sureweld SW-15
  • Welding Process
  • SMAW (Stick)

Classifications

  • Classifications/Approvals

    • ASME SFA 5.1
    • AWS A5.1; E6013

Properties

Typical Properties
As Welded  
Yield Strength 63 ksi, 435 MPa
Tensile Strength 71 ksi, 490 MPa
Reduction in Area 49 %
Elongation in 2" 24 %
Typical Undiluted Weld Metal Analysis  
C 0.06 %
Mn 0.3 %
Si 0.2 %
P 0.012 %
S 0.013 %

SAW

Accessories

Depositions

Deposition Table
Diameter Optimal Amperage Range Amperage Deposition Rate Efficiency
5/64 in, 2.0 mm 50 A 40 - 60 1.4 lbs./hr., 0.6 kg./hr. 73 %
3/32 in, 2.4 mm 85 A 60 - 90 1.6 lbs./hr., 0.7 kg./hr. 73 %
1/8 in, 3.2 mm 125 A 120 - 135 2.1 lbs./hr., 1 kg./hr. 73 %
5/32 in, 4.0 mm 140 A 145 - 190 2.6 lbs./hr., 1.2 kg./hr. 75.6 %
160 A 145 - 190 3 lbs./hr., 1.4 kg./hr. 74.1 %
180 A 145 - 190 3.5 lbs./hr., 1.6 kg./hr. 71.2 %
3/16 in, 4.8 mm 180 A 170 - 230 3.2 lbs./hr., 1.5 kg./hr. 73.9 %
200 A 170 - 230 3.8 lbs./hr., 1.7 kg./hr. 71.1 %
220 A 170 - 230 4.1 lbs./hr., 1.9 kg./hr. 72.9 %
7/32 in, 5.6 mm 250 A 260 - 300 5.3 lbs./hr., 2.4 kg./hr. 71.3 %
270 A 260 - 300 5.7 lbs./hr., 2.6 kg./hr. 73 %
290 A 260 - 300 6.1 lbs./hr., 2.8 kg./hr. 72.7 %
1/4 in, 6.4 mm 290 A 300 - 340 6.2 lbs./hr., 2.8 kg./hr. 75 %
310 A 300 - 340 6.5 lbs./hr., 2.9 kg./hr. 73.5 %
330 A 300 - 340 7.1 lbs./hr., 3.2 kg./hr. 72.1 %