Print this page

LAF 1000

1000 Amp DC Power Source For Submerged Arc Welding

Features

  • Used in conjunction with ESAB PEH or PEI Process Controller
  • Solid state, SCR-controlled, three phase, fancooled DC welding power sources
  • Designed for high productivity mechanized submerged arc or MIG welding
  • Excellent welding characteristics throughout the entire current and voltage range, with particularly good starting and re-ignition properties
  • Extremely efficient power usage saves on power costs
  • Thermal overload protection
  • Extend current range by connecting two power sources in parallel

Classifications

Specifications

LAF 1000
Voltage 3 ph, 60 Hz, 400/440/550 V
Current A 100%, 60 Hz 64/64/52
Fuse, slow A 60 Hz 63
Maximum Load  
@ 100% duty cycle 800 A, 44 V
Setting Range  
MIG/MAG 50-1000 A, 17-45 V
SAW 40-1000 A, 22-45 V
Open circuit voltage 52 V
Open circuit power 145 W
Efficiency 0.84
Power factor 0.95
Enclosure class IP23
Dimensions:  
Length 646 mm, 25 in
Width 552 mm, 22 in
Height 1090 mm, 43 in
Weight 330 kg, 728 lb
Application class S

Ordering Information

Configure this Model

Part No.

LAF 1000
Part No. Model / Product Description UPC
456321881 LAF 1000  

Accessories

There are no accessories.

Extra Info

All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.