A6-MHW Manhole Welder

Equipment designed for welding manholes or nozzles on cyclindrical vessels or flat plates.

Features

  • Equipment designed for welding manholes or nozzles on cyclindrical vessels or flat plates
  • Fix the machine to the workpiece by manual clamping with special jaws to ensure safe constraint of the machine to manholes with diameters between 250-460 mm (10-18 in.)
  • Safety clamping beam with tension bar in the cyclindrical body to prevent tilting
  • Rotation device for the welding head, with a gear wheel drive by the VEC 44 gear-motor with a continuous adjustable speed of 0.1-2.0 rpm
  • Torch moved along a rigid rail by a light-weight carriage
  • Welding head made from A6 components

Classifications

Specifications

A6-MHW Manhole Welder
Welding wire diameters 5/64 to 5/32 in, 2.0 to 4.0 mm
Manhole diameters  
internal minimum 6 in, 150 mm
internal maximum 43 in, 1100 mm
min. wall thickness 2 in, 50 mm
Min. depth necessary for correct clamping on the internal nozzle surface 1 in, 20 mm
Weight 794 lbs, 360 kg