Dual Shield 8100-W es un alambre flexible.
Dual Shield 8100-W es un alambre desarrollado específicamente para unirse con alógenos débiles, aceros con altos grados de efectos de la fuerza como lo son ASTM 588 &242. Dual Shield 8100-W fue diseñado para mezclas de CO2 o Argón / CO2.

| As Welded 75% Ar / 25% CO2 | |
|---|---|
| Yield Strength | 80 ksi, 550 MPa |
| Tensile Strength | 90 ksi, 620 MPa |
| Reduction in Area | 61.2 % |
| Elongation in 2" | 24.0 % |
| As Welded CO2 | |
| Yield Strength | 79 ksi, 545 MPa |
| Tensile Strength | 88 ksi, 605 MPa |
| Reduction in Area | 61.0 % |
| Elongation in 2" | 26.0 % |
| Typical Charpy V-Notch Impact Properties | |
| Testing Temperature 0ºF (-18ºC) | |
| As Welded 75% Ar / 25% CO2 | 39 ft.-lbs., 53 J |
| As Welded CO2 | 34 ft.-lbs., 46 J |
| Testing Temperature -20ºF (-29ºC) | |
| As Welded 75% Ar / 25% CO2 | 34 ft.-lbs., 46 J |
| As Welded CO2 | 24 ft.-lbs., 33 J |
| Typical Undiluted Weld Metal Analysis | |
| 75% Ar / 25% CO2 | |
| C | 0.044 % |
| Mn | 1.01 % |
| Si | 0.62 % |
| P | .012 % |
| S | .010 % |
| Cr | .59 % |
| Ni | 0.60 % |
| Cu | 0.54 % |
| CO2 | |
| C | 0.047 % |
| Mn | .74 % |
| Si | 0.44 % |
| P | .012 % |
| S | .009 % |
| Cr | .54 % |
| Ni | 0.59 % |
| Cu | .50 % |
| Diameter | Amps | Volts | Wire Feed Speed | Deposition Rate | Efficiency |
|---|---|---|---|---|---|
| .045 in, 1.2 mm | 150 A A | 28 | 200 ipm, 508 cm/min | 4.2 lbs./hr., 1.91 kg./hr. | 86 % |
| 210 A A | 29 | 300 ipm, 762 cm/min | 6.3 lbs./hr., 2.86 kg./hr. | 86 % | |
| 250 A A | 30 | 400 ipm, 1016 cm/min | 8.5 lbs./hr., 3.86 kg./hr. | 87 % | |
| 290 A A | 33 | 500 ipm, 1270 cm/min | 10.7 lbs./hr., 4.85 kg./hr. | 87 % | |
| 330 A A | 34 | 600 ipm, 1524 cm/min | 12.7 lbs./hr., 5.76 kg./hr. | 87 % | |
| .052 in, 1.4 mm | 155 A A | 25 | 150 ipm, 381 cm/min | 4.4 lbs./hr., 2 kg./hr. | 87 % |
| 245 A A | 28 | 250 ipm, 635 cm/min | 7.3 lbs./hr., 3.31 kg./hr. | 86 % | |
| 310 A A | 33 | 350 ipm, 889 cm/min | 10.2 lbs./hr., 4.63 kg./hr. | 85 % | |
| 360 A A | 36 | 450 ipm, 1143 cm/min | 13.3 lbs./hr., 6.03 kg./hr. | 85 % | |
| 430 A A | 37 | 600 ipm, 1524 cm/min | 17.6 lbs./hr., 7.98 kg./hr. | 87 % | |
| 1/16 in, 1.6 mm | 190 A A | 27 | 150 ipm, 38 cm/min | 6.1 lbs./hr., 2.77 kg./hr. | 87 % |
| 300 A A | 30 | 250 ipm, 635 cm/min | 10.2 lbs./hr., 4.63 kg./hr. | 87 % |
100% Co2 o Argón / mezclas de CO2.