Sureweld 10P - Plus es un electrodo celulósico para soldadura fuera de posición desarrollado para la industria de soldadura de tuberías. Este electrodo provee una quemadura mas consistente y una quemadura de arco mas indulgente comparado al Sureweld 10P. Produce uniones con calidad rayos "X" en todas posiciones.
| SKU | 811004050 |
|---|---|
| UPC | 662303050368 |
| Model / Product Description | SW 10P PLUS 1/8X14X50#HS |
| Item Weight | 50.00 |
| Min Order | 50 |
| Filler Metal Spec Def | |
| Size | 1/8 , 14 |
| Length | 14 in., 50 in. |
| Weight | 50 lbs., Hermetically Sealed Can lbs. |
| Package | Hermetically Sealed Can |
All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.