El Atom Arc 10018-M es un electrodo E10018-D2 para soldadura fuera de posición bajo en hidrògeno, que se usa en aleaciones bajas, aceros de alta tensiòn dònde se suelda de 100 ksi (690MPa) como minimo de tensiòn requerida.
| SKU | 255091811 |
|---|---|
| UPC | 662303017736 |
| Model / Product Description | AA 10018-MM 1/8X14X50#HS |
| Item Weight | 50.00 |
| Min Order | 50 |
| Filler Metal Spec Def | |
| Size | 1/8 , 14 |
| Length | 14 in., 50 in. |
| Weight | 50 lbs., Hermetically Sealed Can lbs. |
| Package | Hermetically Sealed Can |