Spoolarc 87 HP es un alambre ER70S-7 que figura un rango optimizado manganeso - silicón. Es compatible para soldadura sobre moderadas cantidades de sarro y óxido.
| SKU | 11FTF45 |
|---|---|
| UPC | 662303515225 |
| Model / Product Description | 87HP 035X10LB 12 SP |
| Item Weight | 10.00 |
| Min Order | 10 |
| Filler Metal Spec Def | |
| Size | .035 |
| Length | 10 in. |
| Weight | 10 lbs., Spool lbs. |
| Package | Spool |