Spoolarc Easy Grind es un alambre completamente desoxidado diseñado para la soldadura de los niveles moderados de óxido y pintura y comúnmente usado en los trabajos de reparación de estructuras.
| SKU | 1302F83 |
|---|---|
| UPC | 662303506469 |
| Model / Product Description | EASY GRIND 025X2#SP RANDOM |
| Item Weight | 2.00 |
| Min Order | 2 |
| Filler Metal Spec Def | |
| Size | .025 |
| Weight | 2 lbs. |
| Package | Spool |
All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.