SPOOLARC 83

Spoolarc 83 es un alambre ER80S-D2/ER90S-D2 con 0.5% Mo para proveer alta dureza en el depósito de ambos, las condiciones de soldadura y de esfuerzo.

Ordering Information
SKU1268F74
UPC662303506155
Model / Product Description83 5/32X700#RL
Item Weight700.00
Min Order700
Size5/32
Weight700 lbs.