El coreweld 70 es un cable tubular que contiene ingredientes compresos primordialmente de metales en polvo a todo lo largo incluyendo estabilizadores y elementos de aleación.
| SKU | 243410404 |
|---|---|
| UPC | 662303002497 |
| Model / Product Description | CW 70 045X33#PSP |
| Item Weight | 33.00 |
| Min Order | 33 |
| Filler Metal Spec Def | |
| Size | .045 |
| Length | 33 in. |
| Weight | 33 lbs., Spool lbs. |
| Package | Spool |