Print this page

DUAL SHIELD 7100 Ultra

Dual Shield 7100 Ultra es un alambre con un balance único el cual provee un gran depósito y una gran fundición.

Ordering Information
SKU248000036
UPC662303006792
Model / Product DescriptionDS 7100 ULT 045X10#PSP
Item Weight10.00
Min Order10
Filler Metal Spec Def 
Size.045
Weight10 lbs.
PackageSpool