DUAL SHIELD 7100 Ultra

Dual Shield 7100 Ultra es un alambre con un balance único el cual provee un gran depósito y una gran fundición.

Ordering Information
SKU248000234
UPC662303075545
Model / Product DescriptionDS 7100 ULT 1/16X250#OMP
Item Weight250.00
Min Order2000
Filler Metal Spec Def 
Size1/16
Weight250 lbs.