El Dual Shield II 70 Ultra es un alambre tubular para soldadura fuera de posición, que despliega excepcionales propiedades de impacto cuando es usado con 75% Argón / 25% CO2.
| SKU | 245014857-03 |
|---|---|
| UPC | 662303081621 |
| Model / Product Description | DS II 70 ULT 052X15#PSP |
| Item Weight | 15.00 |
| Min Order | 15 |
| Filler Metal Spec Def | |
| Size | .052 |
| Weight | 15 lbs. |
| Package | Spool |