DUAL SHIELD R-70 Ultra es un alambre tubular que produce poco humo y esta quimicamente balanceado.
| SKU | 242200996 |
|---|---|
| UPC | 662303000264 |
| Model / Product Description | DS R-70 ULT 3/32X600#RL |
| Item Weight | 600.00 |
| Min Order | 600 |
| Filler Metal Spec Def | |
| Size | 3/32 |
| Length | 600 in. |
| Weight | 600 lbs., Reel lbs. |
| Package | Reel |