Print this page

DUAL SHIELD R-70 Ultra

DUAL SHIELD R-70 Ultra es un alambre tubular que produce poco humo y esta quimicamente balanceado.

Ordering Information
SKU242202836
UPC662303001315
Model / Product DescriptionDS R-70 ULT 1/16X500#MP
Item Weight500.00
Min Order500
Size1/16
Weight500 lbs.
PackageMarathon Pack