Print this page

DUAL SHIELD II 81-K2

DUAL SHIELD II 81-K2 es un alambre tubular diseñado para aceros de aleación baja dónde se requiere gran resistencia al impacto de las bajas temperaturas.

Ordering Information
SKU245015102
UPC662303068172
Model / Product DescriptionDS II 81-K2 1/16X300#WR
Item Weight300.00
Min Order900
Filler Metal Spec Def 
Size1/16
Weight300 lbs.
PackageReel