CORESHIELD 8

La soldadura Coreshield 8 es un alambre tubular que presenta características extremadamente buenas de arco, y una apariencia de sueldado.

Ordering Information
SKU242206431
UPC662303072209
Model / Product DescriptionCS 8 5/64X22#AWS VP
Item Weight22.00
Min Order22
Filler Metal Spec Def 
Size5/64
Weight22 lbs.
PackageSpool