SPOOLARC 86

Spoolarc 86 es un alambre ER70S-6 que conttttttienes niveles mas altos de manganeso y silicio que otros grados de alambre de MIG. Provee un charco altamente fluido y una excelente tolerancia de óxido y oxidación (sarro)