SPOOLARC 86

Spoolarc 86 es un alambre ER70S-6 que conttttttienes niveles mas altos de manganeso y silicio que otros grados de alambre de MIG. Provee un charco altamente fluido y una excelente tolerancia de óxido y oxidación (sarro)

Ordering Information
SKU1388F25
UPC662303508289
Model / Product Description86 035X12#SPX48#CT
Item Weight12.00
Min Order12
Size.035
Weight12 lbs.