ALLOY SHIELD 410NiMo

Alloy shield 410 Ni.Mo, es un alambre tubular diseñado para soldar con el proceso dearco sumergido , aleaciones fundidas del tipo 6NM

Ordering Information
SKU258078062
UPC662303008864
Model / Product DescriptionAS 410NIMO 1/8X500#POP
Item Weight500.00
Min Order500
Filler Metal Spec Def 
Size1/8
Weight500 lbs.
PackagePay Off Pack