El Atom Arc 8018-C1 es un electrodo E8018-C1 para soldadura fuera de posición bajo en Hidrógeno el cuál deposita metales con contenidos simbólicos de 2.33% Ni en aplicaciones en las que se requiere rudeza a baja temperatura.
Los electrodos Atom Arc 8018-C1 depositan metales con contenidos simbólicos de 2.33% Ni. Cuyo principal uso es en soldadura de aceros de Nickel-bearing para aplicaciones de baja temeratura en dónde la rudeza de la soldadura es importante a baja temperatura.

| As Welded | |
|---|---|
| Yield Strength | 80 ksi, 550 MPa |
| Tensile Strength | 90 ksi, 620 MPa |
| Elongation in 2" | 30 % |
| Stress Relieved 1 hr. @ 1150ºF (621ºC) | |
| Yield Strength | 75 ksi, 515 MPa |
| Tensile Strength | 86 ksi, 595 MPa |
| Reduction in Area | 74 % |
| Elongation in 2" | 30 % |
| Typical Charpy V-Notch Impact Properties | |
| Testing Temperature -75ºF (-59ºC) | |
| As Welded | 47 ft.-lbs., 64 J |
| Stress Relieved 1 hr. @ 1150ºF (621ºC) | 64 ft.-lbs., 87 J |
| Typical Undiluted Weld Metal Analysis | |
| C | .04 % |
| Mn | 1.1 % |
| Si | .3 % |
| P | 0.011 % |
| S | 0.009 % |
| Ni | 2.4 % |
| Part No. | Model / Product Description | UPC |
|---|---|---|
| 255161416 | AA 8018-C1 1/4X18X50#HS | 662303018146 |
| 255161812 | AA 8018-C1 1/8X14X50#HS | 662303018153 |
| 255163115 | AA 8018-C1 3/16X14X50#HS | 662303018221 |
| 255163214 | AA 8018-C1 3/32X14X50#HS | 662303018252 |
| 255165318 | AA 8018-C1 5/32X14X50#HS | 662303018269 |
| 255167314 | AA 8018-C1 7/32X18X50#HS | 662303018283 |
| 255161820 | AA 8018-C1 1/8X14X10#HS | 662303018160 |
| 255163123 | AA 8018-C1 3/16X14X10#HS | 662303018238 |
| 255163206 | AA 8018-C1 3/32X14X10#HS | 662303018245 |
| 255165326 | AA 8018-C1 5/32X14X10#HS | 662303018276 |
| Diameter | Optimal Amperage | Range Amperage | Deposition Rate | Efficiency |
|---|---|---|---|---|
| 3/32 in, 2.4 mm | 90 A | 70 - 100 | 1.7 lbs./hr., 0.8 kg./hr. | 66.3 % |
| 1/8 in, 3.2 mm | 120 A | 90 - 160 | 2.6 lbs./hr., 1.2 kg./hr. | 71.6 % |
| 140 A | 90 - 160 | 2.7 lbs./hr., 1.2 kg./hr. | 70.9 % | |
| 5/32 in, 4.0 mm | 140 A | 130 - 220 | 3.1 lbs./hr., 1.4 kg./hr. | 75 % |
| 170 A | 130 - 220 | 3.8 lbs./hr., 1.7 kg./hr. | 73.5 % | |
| 3/16 in, 4.8 mm | 200 A | 200 - 300 | 4.9 lbs./hr., 2.2 kg./hr. | 76.4 % |
| 250 A | 200 - 300 | 5.4 lbs./hr., 2.4 kg./hr. | 74.6 % | |
| 7/32 in, 5.6 mm | 250 A | 250 - 350 | 6.5 lbs./hr., 2.9 kg./hr. | 75 % |
| 300 A | 250 - 350 | 7.2 lbs./hr., 3.3 kg./hr. | 74 % | |
| 1/4 in, 6.4 mm | 300 A | 300 - 400 | 7.7 lbs./hr., 3.5 kg./hr. | 78 % |
| 350 A | 300 - 400 | 8.7 lbs./hr., 3.9 kg./hr. | 77 % |
El precalentamiento debe usarse con aceros endurecibles para prevenir el endurecimiento en zonas afectadas por el calor. El precalentamiento puede ser requerido cuando se sueldan secciones pesadas.
All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.