TIGROD ER80S-B2 es una varilla ER80S-B2 TIG que es utilizada para soldar aceros como 0.5% Cr -0.5% Mo, 1% Cr - 0.5% Mo, y 1.25% Cr - 0.5% Mo.
TIGROD ER80S-B2 es una varillas TIG cromo-moly utilizada para unir aceros de resistencia a deformaciones tipos 0.5% Cr - 0.5% Mo, 1% Cr - 0.5% Mo, y 1.25% Cr - 0.5% Mo. Estas varillas revestidas de cobre son primariamente utilizadas para fabricar y reparar tuberias de potencia y boilers en la industria de generación de electricidad.

| Typical Mechanical Properties | |
|---|---|
| Stress Relieved 1 hr. @ 1375ºF (746ºC) GTAW 100% Ar | |
| Yield Strength | 69 ksi, 475 MPa |
| Tensile Strength | 82 ksi, 565 MPa |
| Elongation in 2" | 20 % |
| Typical Wire Analysis | |
| GTAW 100% Ar | |
| C | 0.08 % |
| Mn | 0.6 % |
| Si | 0.6 % |
| P | 0.007 % |
| S | 0.002 % |
| Cr | 1.3 % |
| Mo | 0.5 % |
All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.