TIGROD ER90S-B3 es una varilla ER90S-B3 TIG que es usada para soldar aceros 2.5% Cr - 1% Mo.
TIGROD ER90S-B3 es una varillas TIG cromo-moly utilizada para unir aceros de resistencia a deformaciones tipos 2.5% Cr - 1% Mo. Estas varillas revestidas de cobre son primariamente utilizadas para fabricar y reparar tuberias de potencia y boilers en la industria de generación de electricidad.

| Typical Mechanical Properties | |
|---|---|
| Stress Relieved 1 hr. @ 1375ºF (746ºC) GTAW 100% Ar | |
| Yield Strength | 80 ksi, 555 MPa |
| Tensile Strength | 91 ksi, 625 MPa |
| Elongation in 2" | 19 % |
| Typical Wire Analysis | |
| GTAW 100% Ar | |
| C | 0.08 % |
| Mn | 0.6 % |
| Si | 0.6 % |
| P | 0.007 % |
| S | 0.002 % |
| Cr | 2.25 % |
| Mo | 1 % |