Dual Shield 7100 LC es un alambre el cual tiene un único balance químico que provee un gran depósito y una mejorada productividad al fundir.
Dual Shield 7100 LC es un alambre para uso general al fundir. Esto provee una operación sobresaliente con un arco controlado, mejora la operación a menores niveles de corriente y produce una mínima rebaba la cual se remueve facilmente. Dual Shield 7100 LC puede ser usdo con CO2 ó 75% ar - 25% CO2; CO2 puro es reocomendado cuando la firmeza es fuerte.

| As Welded CO2 | |
|---|---|
| Yield Strength | 79 ksi, 545 MPa |
| Tensile Strength | 89 ksi, 615 MPa |
| Reduction in Area | 52 % |
| Elongation in 2" | 23 % |
| As Welded using 75% Ar - 25% CO2 | |
| Yield Strength | 93 ksi, 640 MPa |
| Tensile Strength | 96 ksi, 660 MPa |
| Reduction in Area | 56 % |
| Elongation in 2" | 25 % |
| Typical Charpy V-Notch Impact Properties | |
| Testing Temperature 0°F (-18°C) | |
| As Welded CO2 | 68 ft - lb, 92 J |
| As Welded 75% Ar - 25% CO2 | 50 ft - lb, 61 J |
| Testing Temperature -20°F (-29°C) | |
| As Welded CO2 | 41 ft - lb, 56 J |
| As Welded 75% Ar - 25% CO2 | 41 ft - lb, 56 J |
| Typical Undiluted Weld Metal Analysis | |
| CO2 | |
| C | 0.03 % |
| Mn | 1.4 % |
| Si | 0.5 % |
| P | 0.010 % |
| Si | 0.010 % |
| 75% Ar / 25% CO2 | |
| C | 0.03 % |
| Mn | 1.6 % |
| Si | 0.6 % |
| P | 0.010 % |
| Si | 0.010 % |
| Part No. | Model / Product Description | UPC |
|---|---|---|
| 248000879 | DS 7100 LC 1/16X33#AWS VP FEMA | 662303076528 |
| 248000895 | DS 7100 LC 045X60#CL | 662303059118 |
| 248000903 | DS 7100 LC 1/16X33#AWS | 662303046057 |
| 248000911 | DS 7100 LC 045X10#PSP | 662303046262 |
| 248000929 | DS 7100 LC 1/16X60#CL | 662303046392 |
| 248000937 | DS 7100 LC 045X33#AWS | 662303048075 |
| 248000945 | DS 7100 LC 1/16X60#CL BK | 662303048099 |
| 248000960 | DS 7100 LC 052X33#AWS | 662303048334 |
| 248000978 | DS 7100 LC 1/16X33#AWS BK | 662303048389 |
| 248000986 | DS 7100 LC 1/16X500#MP | 662303049270 |
| 248000994 | DS 7100 LC 1/16X600#WR | 662303049508 |
| 248001018 | DS 7100 LC 052X10#PSP | 662303049652 |
| 248001026 | DS 7100 LC 045X15#PSP | 662303053208 |
| 248001034 | DS 7100 LC 052X500#MP | 662303058821 |
| 248001042 | DS 7100 LC 052X60#CL | 662303059125 |
| 248001059 | DS 7100 LC 045X500#MP | 662303059156 |
| 248001083 | DS 7100 LC 1/16X600#OMP | 662303076160 |
| 248001091 | DS 7100 LC 052X15#PSP | 662303076306 |
| 248001109 | DS 7100 LC 1/16X15#PSP | 662303076313 |
| 248001117 | DS 7100 LC 045X600#OMP | 662303078546 |
| 248001125 | DS 7100 LC 052X600#OMP | 662303078553 |
| Diameter | Wire Feed Speed | Amps | Volts | Shielding Gas | TTW Dist | Deposition Rate | Efficiency |
|---|---|---|---|---|---|---|---|
| 0.045 in, 1.2 mm | 200 ipm, 508 cm/min | 145 A | 24.5 V | CO2 | 0.625 in. | 3.6 lbs./hr., 1.6 kg./hr. | 81.2 % |
| 300 ipm, 762 cm/min | 190 A | 26 V | CO2 | 0.625 in. | 5.4 lbs./hr., 2.5 kg./hr. | 81.4 % | |
| 400 ipm, 1016 cm/min | 235 A | 27.5 V | CO2 | 0.625 in. | 7.3 lbs./hr., 3.3 kg./hr. | 82.5 % | |
| 500 ipm, 1270 cm/min | 265 A | 29 V | CO2 | 0.625 in. | 9.3 lbs./hr., 4.2 kg./hr. | 82.8 % | |
| 600 ipm, 1524 cm/min | 305 A | 30 V | CO2 | 0.625 in. | 11.3 lbs./hr., 5.1 kg./hr. | 83.7 % | |
| 0.052 in, 1.3 mm | 150 ipm, 381 cm/min | 145 A | 25 V | CO2 | 0.75 in. | 3.4 lbs./hr., 1.5 kg./hr. | 74.3 % |
| 200 ipm, 508 cm/min | 180 A | 25.5 V | CO2 | 0.75 in. | 4.5 lbs./hr., 2.0 kg./hr. | 74.6 % | |
| 300 ipm, 762 cm/min | 235 A | 27.5 V | CO2 | 0.75 in. | 7.0 lbs./hr., 3.2 kg./hr. | 78.2 % | |
| 400 ipm, 1016 cm/min | 285 A | 28.5 V | CO2 | 0.75 in. | 9.8 lbs./hr., 4.4 kg./hr. | 81.3 % | |
| 500 ipm, 1270 cm/min | 230 A | 29.5 V | CO2 | 0.75 in. | 12.2 lbs./hr., 5.5 kg./hr. | 82.3 % | |
| 600 ipm, 1524 cm/min | 370 A | 30.2 V | CO2 | 0.75 in. | 14.7 lbs./hr., 6.7 kg./hr. | 82.7 % | |
| 0.062 in, 1.6 mm | 150 ipm, 381 cm/min | 195 A | 24.5 V | CO2 | 0.75 in. | 4.5 lbs./hr., 2.0 kg./hr. | 73.7 % |
| 250 ipm, 635 cm/min | 285 A | 26 V | CO2 | 0.75 in. | 8.1 lbs./hr., 3.7 kg./hr. | 79.4 % | |
| 300 ipm, 762 cm/min | 320 A | 28 V | CO2 | 0.75 in. | 9.7 lbs./hr., 4.4 kg./hr. | 79.9 % | |
| 350 ipm, 889 cm/min | 345 A | 30 V | CO2 | 0.75 in. | 11.5 lbs./hr., 5.2 kg./hr. | 80.7 % | |
| 400 ipm, 1016 cm/min | 385 A | 32 V | CO2 | 0.75 in. | 13.4 lbs./hr., 6.1 kg./hr. | 82.6 % | |
| 500 ipm, 1270 cm/min | 445 A | 32.5 V | CO2 | 0.75 in. | 16.7 lbs./hr., 7.6 kg./hr. | 82.8 % |
CO2 ó Argón/CO2 hacen hasta 75% Ar.