El Dual Shield Arc 70 es un alambre tubular para soldaduras planas y horizontales con sobrecarga de óxido y cascarillas de laminación.
El Dual Shield Arc 70 es un alambre tubular con soldadura para soldaduras planas y horizontales con sobrecarga de óxido y cascarills de laminación. Las características del Arc y los niveles de salpicado, son extremadamente bajos.

| As Welded CO2 | |
|---|---|
| Yield Strength | 76 ksi, 530 MPa |
| Tensile Strength | 90 ksi, 620 MPa |
| Elongation in 2" | 26 % |
| Typical Charpy V-Notch Inpact Properties | |
| Testing Temperature 0ºF (-18ºC) | |
| As Welded CO2 | 30 ft.-lbs., 41 J |
| Typical Undiluted Weld Metal Analysis | |
| As Welded CO2 | |
| C | 0.07 % |
| Mn | 1.36 % |
| Si | 0.65 % |
| P | 0.016 % |
| S | 0.013 % |
| Part No. | Model / Product Description | UPC |
|---|---|---|
| 245002043 | DS ARC-70 3/32X250#SPOP | 662303075446 |
| 245002001 | DS ARC-70 1/16X60#CL | 662303003678 |
| 245002019 | DS ARC-70 5/64X60#CL | 662303030988 |
| 245002027 | DS ARC-70 3/32X60#CL | 662303003692 |
| 245002035 | DS ARC-70 7/64X60#CL | 662303075460 |
| 245002068 | DS ARC-70 1/16X500#MP | 662303076078 |
| Diameter | Amps | Volts | Wire Feed Speed | Deposition Rate | Efficiency |
|---|---|---|---|---|---|
| 1/16 in, 1.6 mm | 190 A | 27 | 150 ipm, 38 cm/min | 6.1 lbs./hr., 2.77 kg./hr. | 87 % |
| 300 A | 30 | 250 ipm, 635 cm/min | 10.2 lbs./hr., 4.63 kg./hr. | 87 % | |
| 365 A | 33 | 300 ipm, 762 cm/min | 12.3 lbs./hr., 5.58 kg./hr. | 86 % | |
| 410 A | 33 | 350 ipm, 889 cm/min | 14 lbs./hr., 6.35 kg./hr. | 88 % | |
| 450 A | 33 | 400 ipm, 1016 cm/min | 16.1 lbs./hr., 7.3 kg./hr. | 87 % | |
| 500 A | 39 | 500 ipm, 1270 cm/min | 20.1 lbs./hr., 9.11 kg./hr. | 87 % | |
| 5/64 in, 2.0 mm | 250 A | 26 | 112 ipm, 284 cm/min | 6.4 lbs./hr., 2.9 kg./hr. | 85 % |
| 350 A | 28 | 176 ipm, 447 cm/min | 10.5 lbs./hr., 4.76 kg./hr. | 85 % | |
| 450 A | 31 | 258 ipm, 655 cm/min | 14.8 lbs./hr., 6.71 kg./hr. | 85 % | |
| 3/32 in, 2.4 mm | 350 A | 30 | 124 ipm, 315 cm/min | 9.6 lbs./hr., 4.35 kg./hr. | 84 % |
| 400 A | 30 | 166 ipm, 422 cm/min | 12.7 lbs./hr., 5.76 kg./hr. | 85 % | |
| 450 A | 31 | 197 ipm, 500 cm/min | 15 lbs./hr., 6.8 kg./hr. | 86 % | |
| 500 A | 32 | 237 ipm, 602 cm/min | 18.5 lbs./hr., 8.39 kg./hr. | 86 % | |
| 550 A | 34 | 278 ipm, 706 cm/min | 21.3 lbs./hr., 9.66 kg./hr. | 88 % | |
| 7/64 in, 2.8 mm | 550 A | 30 | 140 ipm, 356 cm/min | 17.1 lbs./hr., 7.76 kg./hr. | 85 % |
| 625 A | 34 | 161 ipm, 409 cm/min | 19.6 lbs./hr., 8.89 kg./hr. | 86 % | |
| 700 A | 36 | 190 ipm, 483 cm/min | 23 lbs./hr., 10.43 kg./hr. | 86 % |
CO2
All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.