| As Welded using 75% Ar - 25% CO2 | |
|---|---|
| Tensile Strength | 85 ksi, 580 MPa |
| Yield Strength | 60 ksi, 410 MPa |
| Elongation in 2" | 44 % |
| Typical Undiluted Weld Metal Analysis | |
| 100% CO2 | |
| C | 0.03% |
| Mn | 1.2% |
| Si | 0.8% |
| Cr | 19% |
| Ni | 10% |
| Mo | 0.1% |
| Cu | 0.15% |
| Ferrite | 7 FN |
| 75% Ar / 25% CO2 | |
| C | 0.03% |
| Mn | 1.2% |
| Si | 0.9% |
| Cr | 19% |
| Ni | 10% |
| Mo | 0.1% |
| Cu | 0.15% |
| Ferrite | 7 FN |
| Part No. | Model / Product Description | UPC |
|---|---|---|
| 252200035 | SB 308L 1/16X50#CL | 662303007492 |
| 252200043 | SB 308L 1/16X33#PSP VP | 662303007508 |
| 252200050 | SB 308L 045X33#PSP VP | 662303007515 |
| 252200100 | SB 308L 045X15#PSP VP/60CT | 662303044473 |
| 252200175 | SB 308L 045X10#PSP VP/60CT | 662303007607 |
| 252200423 | SB 308L 035X33#PSP VP | 662303007720 |
| 252200449 | SB 308L 035X10#PSP VP/60CT | 662303007744 |
| 252201769 | SB 308L 1/16X250#SPOP | 662303080051 |
| Diameter | Amps | Volts | Wire Feed Speed | Deposition Rate | Efficiency | Electrical Stickout |
|---|---|---|---|---|---|---|
| .035 in, 0.9 mm | 100 A | 23 | 265 ipm, 6.7 cm/min | 2.9 lbs./hr., 1.3 kg./hr. | 83.9 % | 1/2 - 1 inches, 12.5 - 25 mm |
| 120 A | 23 | 315 ipm, 8 cm/min | 3.4 lbs./hr., 1.5 kg./hr. | 81.4 % | 1/2 - 1 inches, 12.5 - 25 mm | |
| 140 A | 25 | 405 ipm, 10.3 cm/min | 4.6 lbs./hr., 2.1 kg./hr. | 82.6 % | 1/2 - 1 inches, 12.5 - 25 mm | |
| 170 A | 26 | 530 ipm, 13.5 cm/min | 5.7 lbs./hr., 2.6 kg./hr. | 81.8 % | 1/2 - 1 inches, 12.5 - 25 mm | |
| .045 in, 1.2 mm | 130 A | 25 | 227 ipm, 5.8 cm/min | 4.25 lbs./hr., 1.9 kg./hr. | 84 % | 1/2 - 1 inches, 12.5 - 25 mm |
| 165 A | 26 | 341 ipm, 8.7 cm/min | 6.14 lbs./hr., 2.8 kg./hr. | 83 % | 1/2 - 1 inches, 12.5 - 25 mm | |
| 190 A | 28 | 445 ipm, 11.3 cm/min | 8.08 lbs./hr., 3.7 kg./hr. | 84 % | 1/2 - 1 inches, 12.5 - 25 mm | |
| 220 A | 30 | 567 ipm, 14.4 cm/min | 10.24 lbs./hr., 4.6 kg./hr. | 84 % | 1/2 - 1 inches, 12.5 - 25 mm | |
| 1/16 in, 1.6 mm | 170 A | 25 | 154 ipm, 3.9 cm/min | 5.34 lbs./hr., 2.4 kg./hr. | 83 % | 1/2 - 1 inches, 12.5 - 25 mm |
| 210 A | 27 | 193 ipm, 4.9 cm/min | 6.89 lbs./hr., 3.1 kg./hr. | 82.5 % | 1/2 - 1 inches, 12.5 - 25 mm | |
| 250 A | 28 | 243 ipm, 6.2 cm/min | 8.57 lbs./hr., 3.9 kg./hr. | 83 % | 1/2 - 1 inches, 12.5 - 25 mm | |
| 300 A | 29 | 321 ipm, 8.2 cm/min | 11.43 lbs./hr., 5.2 kg./hr. | 83 % | 1/2 - 1 inches, 12.5 - 25 mm |
El Shield-Bright 308L fué desarrollado para soldar aceros inoxidables tipo 304L, pero puede ser usado para otros aceros inoxidables incluyendo los tipos 301, 302 & 304. Puede ser usado exitosamente para soldar aceros inoxidables tipo 321 y 347 provistos con servicio de temperatura a menos de 600ºF (315ºC).
El Shield-Bright 308L fué desarrollado para soldar en toda posición, y rinde particularmente bien en soldadura de posición vertical con excelente remosión de escoria. Puede ser usado con cualquier gas 75% Ar – 25% CO2 gases.
75%Ar / 25%CO2 or 100% CO2
All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.