Print this page

ALL-STATE 1113

Fundente de pasta para brazing a altas temperaturas en hierro fundido, acero templado, níquel, plata y cobre.

características

Fundente de pasta gris para soldadura y brazing en hierro fundido, acero templado, níquel y cobre. Activo a 1400 °F y protege hasta 2200 °F. Se realiza a AWS A5.31, Tipo FB3-G

clasificaciones

propiedades

Typical Properties

Part No.

1113
Part No. Model / Product Description UPC
69080034 A/S BRAZO 1113 FLUX 35# PAIL 662393009796
69080227 A/S 1113 NCK SILVER FLUX 1X1 662393004227

SAW

Accessories

Depositions/Paramaters

Extra Info

Complementary Products

Seismic Data