Fundente para soldadura en acero, hierro fundido, cobre y latón.

características

Fundente de polvo blanco para soldadura en acero, hierro fundido, cobre y latón. Activo desde 1400°F a 2000°F. Se realiza a AWS A5.31 TYPE FB3-F

clasificaciones