Spoolarc 95 es una alambre de alta fuerza de grado militar usado para la soldadura de los aceros HY-80
Spoolarc 95 es una alambre de alta fuerza de grado militar usado para la soldadura de los aceros HY-80
Las aplicaciones del Spoolarc 95 incluyen los tanques militares, barcos y submarinos.

| Yield Strength | 95,000 ksi, 655 MPa |
|---|---|
| Tensile Strength | 105,000 ksi, 725 MPa |
| Elongation in 2" | 23 % |
| Typical Charpy V-Notch Impact Properties | |
| Testing Temperature 0°F (-18°C) | 93 ft.-lbs., 126 J |
| Testing Temperature -60ºF (-51ºC) | 65 ft.-lbs., 88 J |
| Typical Undiluted Weld Metal Analysis | |
| C | 0.07 % |
| Mn | 1.40 % |
| Si | 0.35 % |
| P | 0.008 % |
| S | 0.007 % |
| Cr | 0.20 % |
| Ni | 1.80 % |
| Mo | 0.35 % |
| Part No. | Model / Product Description | UPC |
|---|---|---|
| 2296F10 | 95 CU 3/32X800#DR | 662303668563 |
| 2296F14 | 95 CU 5/32X800#DR | 662303514778 |
| 229DF08 | 95 CU 1/16X36 F1 MIL | 662303668549 |
| 2291F10 | 95 CU 3/32X36 | 662303510916 |
| 2291F12 | 95 CU 1/8X36 | 662303510923 |
| 2294F30 | 95 CU 3/32X65#CL | 662303510978 |
| 2294F32 | 95 CU 1/8X65#CL | 662303510985 |
| 2294F34 | 95 CU 5/32X65#CL | 662303510992 |
| 2295F32 | 95 CU 1/8X200#CL | 662303523176 |
| 2298F65 | 95 CU 035X35#SP | 662303520410 |
| 2298F66 | 95 CU 040X35#SP | 662303668280 |
| 2298F67 | 95 CU 045X35#SP | 662303511043 |
| 2298F68 | 95 CU 1/16X35#SP | 662303520403 |
| 229DF28 | 95 CU 1/16X36 F2 MIL | 000000000000 |
| 229DF48 | 95 CU 1/16X18X20#CT F1 MIL | 662303521677 |
| 229DF50 | 95 CU 3/32X18 S/C MIL F1 | 662303520311 |
| 229DF68 | 95 CU 1/16X12X10#CT F1 MIL | 662303511104 |
| 229EFBC | 95 CU 035X25#SP MIL | 662303668495 |
| 229EFBD | 95 CU 035X35#SP MIL | 662303511128 |
| 229EFBS | 95 CU 035X11#SP MIL | 662303522483 |
| 229EFDC | 95 CU 045X25#SP MIL | 662303520236 |
| 229EFDD | 95 CU 045X35#SP MIL | 662303511142 |
| 229EFDS | 95 CU 045X11#SP MIL | 662303520151 |
| 229EFDSBI | 95 CU 045X11#SP/44# MIL BATH | 662303523183 |
| 229EFDY | 95 CU 045X60#SP MIL | 662303511159 |
| 229EFEC | 95 CU 1/16X25#SP MIL | 662303668679 |
| 229EFED | 95 CU 1/16X35#SP MIL | 662303511173 |
| 229EFGD | 95 CU 3/32X35#SP MIL | 662303511197 |
| 229EFGE | 95 CU 3/32X65#CL MIL | 662303668624 |
| 229EFHE | 95 CU 1/8X65#CL MIL | 662303668242 |
| 229EFHEBI | 95 CU 1/8X65#CL MIL BATH | 662303668556 |
| 229EFJE | 95 CU 5/32X65#CL MIL | 662303668037 |
| 2312F28 | 95 BARE 1/16X35#SP | 662303511272 |
| 231EFHE | 95 BARE 1/8X65#CL MIL | 662303512644 |
| 231EFHEBI | 95 BARE 1/8X65#CL MIL BATH | 662303523244 |
| Diameter | Amps | Deposition Rate | Average Deposition Efficiency |
|---|---|---|---|
| 1/16 in, 1.6 mm | 400 | 13.0 lbs./hr., 5.90 kg./hr. | 99 % |
| 500 | 17.0 lbs./hr., 7.71 kg./hr. | 99 % | |
| 5/64 in, 2.0 mm | 300 | 10.8 lbs./hr., 4.90 kg./hr. | 99 % |
| 400 | 14.5 lbs./hr., 6.58 kg./hr. | 99 % | |
| 500 | 18.2 lbs./hr., 8.26 kg./hr. | 99 % | |
| 3/32 in, 2.4 mm | 400 | 13.2 lbs./hr., 5.99 kg./hr. | 99 % |
| 500 | 17.0 lbs./hr., 7.71 kg./hr. | 99 % | |
| 600 | 22.0 lbs./hr., 9.98 kg./hr. | 99 % | |
| 1/8 in, 3.2 mm | 400 | 11.0 lbs./hr., 4.99 kg./hr. | 99 % |
| 500 | 14.5 lbs./hr., 6.58 kg./hr. | 99 % | |
| 600 | 18.0 lbs./hr., 8.16 kg./hr. | 99 % | |
| 700 | 21.2 lbs./hr., 9.62 kg./hr. | 99 % | |
| 5/32 in, 4.0 mm | 500 | 12.5 lbs./hr., 5.67 kg./hr. | 99 % |
| 600 | 16.0 lbs./hr., 7.26 kg./hr. | 99 % | |
| 700 | 19.5 lbs./hr., 8.85 kg./hr. | 99 % | |
| 800 | 23.0 lbs./hr., 10.43 kg./hr. | 99 % | |
| 900 | 26.0 lbs./hr., 11.79 kg./hr. | 99 % | |
| 3/16 in, 4.8 mm | 600 | 13.9 lbs./hr., 6.31 kg./hr. | 99 % |
| 700 | 17.5 lbs./hr., 7.94 kg./hr. | 99 % | |
| 800 | 21.0 lbs./hr., 9.53 kg./hr. | 99 % | |
| 900 | 25.0 lbs./hr., 11.34 kg./hr. | 99 % | |
| 1000 | 29.2 lbs./hr., 13.25 kg./hr. | 99 % | |
| 1100 | 34.0 lbs./hr., 15.42 kg./hr. | 99 % |
| Diameter | Wire Feed Speed | Amps | Volts | Deposition Rate |
|---|---|---|---|---|
| .023 in, 0.6 mm | 150 ipm, 381 cm/min | 45 | 14 | 1 lbs./hr., 0.4 kg./hr. |
| 200 ipm, 508 cm/min | 55 | 14 | 1.3 lbs./hr., 0.6 kg./hr. | |
| 250 ipm, 635 cm/min | 65 | 15 | 1.6 lbs./hr., 0.7 kg./hr. | |
| 300 ipm, 762 cm/min | 74 | 15 | 2 lbs./hr., 0.9 kg./hr. | |
| 350 ipm, 889 cm/min | 84 | 16 | 2.3 lbs./hr., 1 kg./hr. | |
| 380 ipm, 965 cm/min | 90 | 16 | 2.5 lbs./hr., 1.1 kg./hr. | |
| .030 in, 0.8 mm | 150 ipm, 381 cm/min | 60 | 14 | 1.7 lbs./hr., 0.8 kg./hr. |
| 200 ipm, 508 cm/min | 80 | 15 | 2.2 lbs./hr., 1 kg./hr. | |
| 250 ipm, 635 cm/min | 100 | 15 | 2.8 lbs./hr., 1.3 kg./hr. | |
| 300 ipm, 762 cm/min | 120 | 16 | 3.3 lbs./hr., 1.5 kg./hr. | |
| 350 ipm, 889 cm/min | 140 | 16 | 3.9 lbs./hr., 1.8 kg./hr. | |
| 360 ipm, 914 cm/min | 144 | 16 | 4 lbs./hr., 1.8 kg./hr. | |
| .035 in, 0.9 mm | 180 ipm, 457 cm/min | 90 | 15 | 2.7 lbs./hr., 1.2 kg./hr. |
| 220 ipm, 559 cm/min | 113 | 16 | 3.3 lbs./hr., 1.5 kg./hr. | |
| 260 ipm, 660 cm/min | 137 | 18 | 4 lbs./hr., 1.8 kg./hr. | |
| 300 ipm, 762 cm/min | 160 | 19 | 4.6 lbs./hr., 2.1 kg./hr. | |
| .045 in, 1.2 mm | 125 ipm, 318 cm/min | 130 | 17 | 3.1 lbs./hr., 1.4 kg./hr. |
| 160 ipm, 406 cm/min | 163 | 18 | 4 lbs./hr., 1.8 kg./hr. | |
| 200 ipm, 508 cm/min | 200 | 19 | 5 lbs./hr., 2.3 kg./hr. | |
| .052 in, 1.3 mm | 135 ipm, 343 cm/min | 150 | 17 | 4.5 lbs./hr., 2.1 kg./hr. |
| 190 ipm, 483 cm/min | 200 | 20 | 6.4 lbs./hr., 2.9 kg./hr. | |
| 160 ipm, 406 cm/min | 173 | 18 | 5.4 lbs./hr., 2.4 kg./hr. |
Diseñado para la soldadura sencilla o multipase donde la alta resistencia y la tenacidad del impacto. Es primordialmente para los aceros del grado militar así como los HY-80. Este alambre cumple las especificaciones del tipo militar 100S-1, MIL-E-23765/2. Las aplicaciones incluyendo los tanques militares, barcos, etc. Utilizable con el fundente OK 10.62
All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.