Print this page

Dual Shield 710X

Dual Shield 710X is an all-position flux cored wire that offers outstanding operator appeal with an easily controlled arc, improved operation at both lower and higher current levels, minimal spatter and easily removed slag. It is tested and certified to meet the new AWS A5.20 ‘D’ designation requirements, making this gas-shielded wire an excellent choice for demand critical welds when FEMA 353, D1.1 or D1.8 Seismic Supplement is utilized.

características

Dual Shield 710X is an all-position flux cored wire for general purpose welding. It provides outstanding operator appeal with an easily controlled arc, improved operation at both lower and higher current levels, minimal spatter and easily removed slag. Dual Shield 710X can be used with either 100% CO2 or a 75/25 Argon CO2 gas mix, however pure CO2 is recommended in applications where weld joint restraint is high.

Applications include rail car, barges, civil construction, light equipment and general fabrication.

Please see Related Links on the right side of this page to download the Seismic Data Sheet and Seismic Certifications.

Dual Shield 710X
  • Industry
  • Carro de ferrocarril
  • Astillero
  • Fabricación en general
  • Barges
  • Light Equipment
  • Construcción civil
  • Welding Process
  • Soldadura con alambre tubular de alimentación continua

clasificaciones

  • Classifications/Approvals

    • Seismic Certified "D"
    • L.R. - 3S,3YS
    • DNV III YMS
    • ABS - 3SA, 3YSA
    • AWS A5.20; E71T-9C/T-9M
    • CERTIFIED BY C.W.B.- CSA W48
    • AWS A5.20; E71T-1C/T-1M
    • ASME SFA 5.20

propiedades

Typical Properties
As Welded  
Shielding Gas CO2
Yield Strength 75 ksi, 520 MPa
Tensile Strength 87 ksi, 625 MPa
Elongation (In 2", 51 mm) 28 %
As Welded  
Shielding Gas 75/25
Yield Strength 83 ksi, 570 MPa
Tensile Strength 93 ksi, 640 MPa
Elongation (In 2", 51 mm) 27 %
Typical Charpy V-Notch Impact Properties  
Shielding Gas CO2
Testing Temperature  
0°F (-18°C) 57 ft. - lbs., 77 J
-20°F (-29°C) 49 ft. - lbs., 66 J
Shielding Gas 75/25
Testing Temperature  
0°F (-18°F) 75 ft. - lbs., 102 J
-20°F (-29°C) 50 ft. - lbs., 68 J
Typical Undiluted Weld Metal Analysis (%)  
Shielding Gas CO2
C 0.03
Mn 1.4
Si 0.5
P 0.007
S 0.009
Ni 0.4
Shielding Gas 75/25
C 0.03
Mn 1.5
Si 0.6
P 0.005
S 0.009
Ni 0.4

Part No.

710X
Part No. Model / Product Description UPC
245019369 DS 710X 1/16X15#PSP 662303084011
245019351 DS 710X 052X15#PSP 662303084004
245019344 DS 710X 045X15#PSP 662303083977
245019336 DS 710X 052X600#OMP 662303083823
245019328 DS 710X 1/16X600#OMP 662303083519
245019310 DS 710X 045X600#OMP 662303083502
245019302 DS 710X 1/16X60#CL 662303083489
245019294 DS 710X 045X60#CL 662303083472
245019286 DS 710X 052X60#CL 662303083205
245019252 DS 710X 045X33#AWS 662303082147
245019260 DS 710X 052X33#AWS 662303082154
245019278 DS 710X 1/16X33#AWS 662303082161

SAW

Accessories

Depositions/Paramaters

Deposition Table Gas: CO2
Diameter Amperage Voltage Wire Feed Speed Deposition Rate Efficiency Rate TTW
0.045 in. 126 A 22 V 160 ipm 2.8 lbs/hr 81 % 3/4"
140 A 23 V 190 ipm 3.3 lbs/hr 81 % 3/4"
154 A 23 V 220 ipm 3.9 lbs/hr 81 % 3/4"
167 A 24 V 250 ipm 4.5 lbs/hr 82 % 3/4"
180 A 24 V 280 ipm 5.1 lbs/hr 82 % 3/4"
193 A 25 V 310 ipm 5.6 lbs/hr 82 % 3/4"
205 A 26 V 340 ipm 6.2 lbs/hr 83 % 3/4"
217 A 26 V 370 ipm 6.8 lbs/hr 83 % 3/4"
0.052 in. 153 A 24 V 160 ipm 4.0 lbs/hr 81 % 3/4"
159 A 24 V 170 ipm 4.3 lbs/hr 81 % 3/4"
166 A 25 V 180 ipm 4.5 lbs/hr 81 % 3/4"
172 A 25 V 190 ipm 4.8 lbs/hr 81 % 3/4"
178 A 25 V 200 ipm 5.0 lbs/hr 81 % 3/4"
184 A 25 V 210 ipm 5.3 lbs/hr 81 % 3/4"
190 A 26 V 220 ipm 5.5 lbs/hr 81 % 3/4"
196 A 26 V 230 ipm 5.8 lbs/hr 82 % 3/4"
201 A 26 V 240 ipm 6.0 lbs/hr 82 % 3/4"
207 A 26 V 250 ipm 6.3 lbs/hr 82 % 3/4"
1/16 in. 149 A 23 V 100 ipm 2.8 lbs/hr 80 % 3/4"
168 A 24 V 120 ipm 3.5 lbs/hr 80 % 3/4"
187 A 24 V 140 ipm 4.2 lbs/hr 80 % 3/4"
205 A 25 V 160 ipm 4.9 lbs/hr 80 % 3/4"
223 A 25 V 180 ipm 5.6 lbs/hr 80 % 3/4"
240 A 25 V 200 ipm 6.3 lbs/hr 80 % 3/4"
257 A 26 V 220 ipm 7.0 lbs/hr 81 % 3/4"
273 A 26 V 240 ipm 7.7 lbs/hr 81 % 3/4"
289 A 26 V 260 ipm 8.4 lbs/hr 81 % 3/4"
Deposition Table Gas: 75/25
Diameter Amperage Voltage Wire Feed Speed Deposition TTW
0.045 in. 110 A 19.0 V 150 ipm 1/2" - 1"
123 A 19.8 V 180 ipm 1/2" - 1"
136 A 20.5 V 210 ipm 1/2" - 1"
149 A 21.3 V 240 ipm 1/2" - 1"
162 A 22.0 V 270 ipm 1/2" - 1"
175 A 22.8 V 300 ipm 1/2" - 1"
188 A 23.5 V 330 ipm 1/2" - 1"
201 A 24.3 V 360 ipm 1/2" - 1"
214 A 25.0 V 390 ipm 1/2" - 1"
227 A 25.8 V 420 ipm 1/2" - 1"
240 A 26.5 V 450 ipm 8.6 lbs./hr. 1/2" - 1"
0.052 in. 150 A 20.0 V 150 ipm 1/2" - 1"
162 A 20.7 V 180 ipm 1/2" - 1"
173 A 21.3 V 210 ipm 1/2" - 1"
185 A 22.0 V 240 ipm 1/2" - 1"
196 A 22.6 V 270 ipm 1/2" - 1"
208 A 23.3 V 300 ipm 1/2" - 1"
219 A 23.9 V 330 ipm 1/2" - 1"
231 A 24.6 V 360 ipm 1/2" - 1"
242 A 25.2 V 390 ipm 1/2" - 1"
254 A 25.9 V 420 ipm 1/2" - 1"
265 A 26.9 V 450 ipm 8.8 lbs./hr. 1/2" - 1"
1/16 in. 160 A 20.0 V 120 ipm 1/2" - 1"
173 A 20.7 V 135 ipm 1/2" - 1"
185 A 21.3 V 150 ipm 1/2" - 1"
198 A 22.0 V 165 ipm 1/2" - 1"
210 A 22.6 V 180 ipm 1/2" - 1"
223 A 23.3 V 195 ipm 1/2" - 1"
235 A 23.9 V 210 ipm 1/2" - 1"
248 A 24.6 V 225 ipm 1/2" - 1"
260 A 25.2 V 240 ipm 1/2" - 1"
273 A 25.9 V 255 ipm 1/2" - 1"
285 A 26.5 V 270 ipm 9.2 lbs/hr. 1/2" - 1"

Extra Info

DCEP

Complementary Products

Seismic Data