Print this page

Dual Shield II 712X

Dual Shield II 712X is an all-position mixed gas flux cored wire intended for applications requiring outstanding weld metal toughness.

características

Dual Shield II 712X is an all-position flux cored wire intended for applications requiring outstanding weld metal toughness. This X Series wire, in combination with 75% Argon/25% CO2 shielding gas, can produce Charpy V-notch impact results of more than 50 ft.-lbs. (68 J) at -60°F (-51°C) and Crack Tip Opening Displacement (CTOD) results of more than 20 mils (0.5 mm) at -40°F (-40°C). Dual Shield II 712X also provides the smooth arc and low spatter levels characteristic of Dual Shield flux cored wires.

Applications include off-shore oil components, shipbuilding and heavy equipment where exceptional Charpy impact/low temperature toughness is required.

Dual Shield II 712X
  • Industry
  • Heavy Equipment
  • Astillero
  • Offshore Oil
  • Welding Process
  • Soldadura con alambre tubular de alimentación continua

clasificaciones

  • Classifications/Approvals

    • D.N.V. - IV YS
    • AWS A5.20; E71T-1MJ/T-12MJ
    • A.B.S. - 3SA, 4YSA
    • L.R. - 4YS,40S
    • ASME SFA 5.20
    • CERTIFIED BY C.W.B.- CSA W48

propiedades

Typical Properties
As Welded  
Shielding Gas 75/25
Yield Strength 78 ksi, 540 MPa
Tensile Strength 83 ksi, 570 MPa
Elongation (In 2", 51 mm) 28 %
Typical Charpy V-Notch Impact Properties  
Shielding Gas 75/25
Testing Temperature  
0°F (-18°C) 129 ft. - lbs., 175 J
-40°F (-40°C) 93 ft. - lbs., 126 J
Typical Undiluted Weld Metal Analysis (%)  
Shielding Gas 75/25
C 0.05
Mn 1.1
Si 0.3
P 0.009
S 0.010

Part No.

712X
Part No. Model / Product Description UPC
245019757 DS II 712X 045X33#AWS 662303082178
245019765 DS II 712X 052X33#AWS 662303082185
245019773 DS II 712X 1/16X33#AWS 662303082192

SAW

Accessories

Depositions/Paramaters

Deposition Table Gas: 75/25
Diameter Amperage Voltage Wire Feed Speed Deposition TTW
0.045 in. 129 A 19.5 V 160 ipm 1/2"-1"
141 A 20.2 V 190 ipm 1/2"-1"
153 A 20.9 V 219 ipm 1/2"-1"
165 A 21.6 V 249 ipm 1/2"-1"
177 A 22.3 V 278 ipm 1/2"-1"
189 A 23.0 V 308 ipm 1/2"-1"
200 A 23.7 V 337 ipm 1/2"-1"
212 A 24.4 V 367 ipm 1/2"-1"
224 A 25.1 V 396 ipm 1/2"-1"
236 A 25.8 V 426 ipm 1/2"-1"
248 A 26.5 V 455 ipm 9.3 lbs./hr. 1/2"-1"
0.052 in. 135 A 20.0 V 130 ipm 1/2"-1"
148 A 20.6 V 153 ipm 1/2"-1"
160 A 21.1 V 176 ipm 1/2"-1"
173 A 21.7 V 199 ipm 1/2"-1"
185 A 22.2 V 222 ipm 1/2"-1"
198 A 22.8 V 245 ipm 1/2"-1"
210 A 23.3 V 268 ipm 1/2"-1"
223 A 23.9 V 291 ipm 1/2"-1"
235 A 24.4 V 314 ipm 1/2"-1"
248 A 25.0 V 337 ipm 1/2"-1"
260 A 25.5 V 360 ipm 9.4 lbs./hr. 1/2"-1"
1/16 in. 141 A 23.0 V 100 ipm 1/2"-1"
159 A 23.3 V 115 ipm 1/2"-1"
177 A 23.5 V 130 ipm 1/2"-1"
195 A 23.8 V 145 ipm 1/2"-1"
213 A 24.0 V 160 ipm 1/2"-1"
231 A 24.3 V 175 ipm 1/2"-1"
249 A 24.5 V 190 ipm 1/2"-1"
267 A 24.8 V 205 ipm 1/2"-1"
285 A 25.0 V 220 ipm 1/2"-1"
303 A 25.3 V 235 ipm 1/2"-1"
321 A 25.5 V 250 ipm 9.6 lbs./hr. 1/2"-1"