OK Autrod 308L

OK Autrod 308L is a low carbon, stainless wire designed for submerged arc welding of austenitic steels, such as AISI 301, 304, 304L. OK Autrod 308L can be used in combination with OK Flux 10.93 and 10.94.

características

OK Autrod 308L is a continuous, solid, corrosion-resistant, chromium-nickel wire. OK Autrod 308L has good general corrosion resistance. The alloy has a low carbon content which makes it particularly recommended where there is a risk of intergranular corrosion.

Ok Autrod 308L SAW - Web Image Medium
  • Industry
  • Pressure Vessel
  • Fabricación en general
  • Petroquímica
  • Proceso
  • Welding Process
  • Soldadura con Arco Sumergido

clasificaciones

  • Classifications/Approvals

    • ASME IX F No. 6
    • ASME II SFA 5.9 ER308/308L

propiedades

Typical Properties
C <0.03 %
Mn 1.8 %
Si 0.5 %
Cr 20.3 %
Ni 10.0 %
Mo <0.3 %
Cu <0.3 %