Arcaloy ER308L is a low carbon grade of 308 designed for MIG or SAW of stainless steels such as AISI 301, 304, 304L steels. Arcaloy ER308L can be used in combination with OK Flux 10.93, 10.94 and 10.95.

características

Arcaloy ER308L may be used successfully for welding types 321 and 347 steels, provided the service temperature is below approximate 700°F (371°C).

  • Industry
  • Astillero
  • Automotriz
  • Fabricación en general
  • Alimentos y bebidas
  • Proceso
  • Welding Process
  • Soldadura con Arco Sumergido

clasificaciones

  • Classifications/Approvals

    • ASME IX F No. 6
    • ASME II SFA 5.9 ER308/308L
    • CWB
    • ABS

propiedades

Typical Properties
C 0.015 %
Mn 1.7 %
Si 0.45 %
S 0.01 %
Cr 20 %
Ni 10 %
Mo 0.1 %
Cu 0.15 %
Ferrita 9 FN