OK Autrod 309L

OK Autrod 309L is a continuous, solid, corrosion-resisting chromium-nickel wire for joining stainless steels to non-alloy or low alloy steels as well as welding of austenitic stainless alloys of 24% Cr, 13% Ni types. OK Autrod 309L can be used in combination with OK Flux 10.93 or 10.94.

características

OK Autrod 309L has good general corrosion resistance. When used for joining dissimilar materials, the corrosion resistance is of secondary importance.

OK Autrod 309L SAW - Web Image Medium
  • Industry
  • Pressure Vessel
  • Fabricación en general
  • Proceso
  • Welding Process
  • Soldadura con Arco Sumergido

clasificaciones

  • Classifications/Approvals

    • ASME II SFA 5.9 ER309/309L
    • ASME IX F No. 6

propiedades

Typical Properties
C <0.03 %
Mn 1.8 %
Si 0.5 %
Cr 24.0 %
Ni 13.0 %
Mo <0.3 %
Cu <0.3 %