Arcaloy ER309L

Arcaloy ER309L is a continuous, solid, corrosion-resisting chromium-nickel wire for joining stainless steels to non-alloy or low alloy steels as well as welding of austenitic stainless alloys of 24% Cr, 13% Ni types. Arcaloy ER309L can be used in combination with OK Flux 10.93 or 10.94.

características

Arcaloy ER309L has good general corrosion resistance. When used for joining dissimilar materials, the corrosion resistance is of secondary importance.

  • Industry
  • Astillero
  • Proceso
  • Fabricación en general
  • Automotriz
  • Welding Process
  • Soldadura con Arco Sumergido

clasificaciones

  • Classifications/Approvals

    • ASME IX F No. 6
    • ABS
    • CWB
    • ASME II SFA 5.9 ER309/309L

propiedades

Typical Properties
C 0.21 %
Mn 1.75 %
Si .51 %
P 0.0.14 %
S 0.006 %
Cr 23.40 %
Ni 12.70 %
Mo .1 %
N 0.05 %