OK Band 317L

OK Band 317L is a stainless welding strip designed for cladding using the submerged arc welding process. Band 309L together with OK Flux 10.05 and Band 317L produces a 317L deposit.

características

OK Band 317L was formally known as OK Band 11.67.

OK Band 317L - Web Image Medium
  • Industry
  • Pressure Vessel
  • Petroquímica
  • Welding Process
  • Soldadura con Arco Sumergido

clasificaciones

  • Classifications/Approvals

    • SFA/AWS A5.9 EQ317L

propiedades

Typical Properties
Typical Strip Analysis  
C 0.03 %
Si 0.65 %
Mn 2 %
Cr 20 %
Ni 15 %
Mo 4 %

Part No.

SAW

Accessories

Depositions/Paramaters

Recommended Welding Parameters and Deposition Data
Amps Volts Welding Parameters Deposition Rate
750 A28 V5 (12) in/min (cm/min)31 (14) lbs/h (kg/h), 345 (0.23) inch²/h (m²/h)