Alloy Shield 30S

Alloy Shield 30S is composite metal cored subarc wire designed to be used for build-up and for hardfacing applications where moderate hardness and good machinability are important. Designed to be used with 601 Flux.

características

Alloy Shield 30S is commonly used to build up a base to support the final overlay, for example, in a steel mill concast roll rebuild application. Nominal all weld metal harness is 30Rc.

Alloy Shield 30S - Web Image Medium
  • Welding Process
  • Soldadura con Arco Sumergido

clasificaciones

propiedades

Typical Properties
Alloy Shield 30S  
Typical Mechancial Properties  
As Welded with OK Flux 601, 3 layers on 1045 steel  
Hardness 28 Rc