Arcaloy ER317L

OK Autrod 2209 (16.86) is a continuous, solid, corrosion-resistant, duplex wire for welding austenitic-ferritic stainless alloys of the 22% Cr, 5% Ni, 3% Mo type. OK Autrod 2209 can be used in combination with OK Flux 10.93.

características

Arcaloy ER317L has a good resistance to general corrosion and pitting due to its high content of molybdenum. The alloy has a low carbon content which makes this alloy particularly recommended were there is a risk of intergranular corrosion. This alloy is used in severe corrosion conditions such as petrochemical and paper industries.

  • Industry
  • Proceso
  • Petroquímica
  • Fabricación en general
  • Papel y pulpa
  • Welding Process
  • Soldadura con Arco Sumergido

clasificaciones

  • Classifications/Approvals

    • ASME SFA 5.9

propiedades

Typical Properties
C 0.17 %
Mn 1.66 %
Si .44 %
Cr 19.4 %
Ni 13.85 %
Mo 3.25 %
N 0.04 %