OK Tigrod 308LSi has good general corrosion resistance. This high silicon Tigrod improves the welding properties such as wetting.

| Yield Strength | 74 ksi, 510 MPa |
|---|---|
| Tensile Strength | 81 ksi, 555 MPa |
| Elongation in 2" | 36 % |
| Typical Charpy V-Notch Impact Properties | |
| Testing Temperature -76°F (-60°C) | 111 ft.-lbs, 150 J |
| Testing Temperature -166°F (-110°C) | 103 ft.-lbs, 140 J |
| Testing Temperature -320ºF (-196ºC) | 74 ft.-lbs., 100 J |
| Testing Temperature 68ºF (20ºC) | 125 ft.-lbs., 170 J |
| Typical wire analysis | |
| C | <0.03 % |
| Mn | 1.8 % |
| Si | 0.8 % |
| Cr | 20.3 % |
| Ni | 10.0 % |
| Mo | <0.3 % |
| Cu | <0.3 % |
| Part No. | Model / Product Description | UPC |
|---|---|---|
| 161216R15A | ES OK ER308LSI 1/16X39X11 E2 | 000000000000 |
| 161224R15A | ES OK ER308LSI 3/32X39X11 E2 | 662303077648 |
| 161232R15A | ES OK ER308LSI 1/8X39X11 E2 | 000000000000 |
| 161240R15A | ES OK ER308LSI 5/32X39X11 E2 | 000000000000 |