Arcaloy ER347 es un acero inoxidable estabilizado columbium para los tipos 347 y 321 de la soldadura inoxidables.
Arcaloy ER347 es diseñado para los tipos 321 y 347 de la soldadura, cuando la temperatura del servicio está debajo de 600°F (316°C). Utilizado donde las condiciones del servicio requieren resistencia máxima a la corrosión.

| GTAW using 100% Argon | |
|---|---|
| Límite elástico | 65 ksi, 450 MPa |
| Resistencia a la tensión | 100 ksi, 690 MPa |
| Elongación en 2" | 45 % |
| Analisis quimico tipico | |
| C | 0.03 % |
| Mn | 1.5 % |
| Si | 0.4 % |
| Cr | 19.5 % |
| Ni | 9.5 % |
| Mo | 0.1 % |
| Cu | 0.1 % |
| Nb | 0.5 % |
| Ferrita | 10 FN |
| Part No. | Model / Product Description | UPC |
|---|---|---|
| 258093525 | AB ER347 035X33#PSP | 662303076597 |
| 256073156 | AB ER347 1/16X36X10T/30CT INK | 662303049201 |
| 256073164 | AB ER347 3/32X36X10T/30CT INK | 662303049218 |
| 256073172 | AB ER347 1/8X36X10T/30CT INK | 662303049225 |
| 258091115 | AB ER347 1/16X33#PSP | 662303027919 |
| 258093517 | AB ER347 035X33#BAWS | 662303027896 |
| 258094515 | AB ER347 045X33#BAWS | 662303027902 |
| 259600807 | AB ER347 1/16X36X10#CT F2 | 662303522711 |
| 259601672 | AB ER347 1/8X36X10#CT F2 | 662303519766 |
| 259601680 | AB ER347 1/8X36X10#CT F1 | 662303030032 |
| Diameter | Wire Feed Speed | DCEP (Electrode Positive) | Volts | Deposition Rate |
|---|---|---|---|---|
| .030 in., 0.8 mm | 156-312 ipm, 396-792 cm/min | 40-120 | 15-20 | 1.4-3.8 lbs./hr., 0.64-1.72 kg./hr |
| .035 in., 0.9 mm | 156-312 ipm, 396-792 cm/min | 60-140 | 15-21 | 1.6-5.4 lbs./hr., 0.73-2.45 kg./hr |
| .045 in., 1.2 mm | 140-280 ipm, 356-711 cm/min | 100-210 | 17-22 | 2.4-6.0 lbs./hr., 1.09-2.72 kg./hr |
| Diameter | Wire Feed Speed | DCEP (Electrode Positive) | Volts | Deposition Rate |
|---|---|---|---|---|
| .030 in., 0.8 mm | 265-550 ipm, 673-1397 cm/min | 160-210 | 24-28 | 6.5-9.6 lbs./hr., 2.95-4.35 kg./hr. |
| .035 in., 0.9 mm | 240-468 ipm, 610-1189 cm/min | 170-255 | 24-30 | 7.8-12.7 lbs./hr., 3.54-5.76 kg./hr. |
| .045 in., 1.2 mm | 192-360 ipm, 488-914 cm/min | 200-300 | 24-30 | 6.8-13.6 lbs./hr., 3.08-6.17 kg./hr. |
| .062 in., 1.6 mm | 120-192 ipm, 305-488 cm/min | 215-325 | 24-32 | 7.3-14.5 lbs./hr., 3.31-6.58 kg./hr. |
All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.