Print this page

Ok Autrod 16.95

OK Autrod 16.95 (307Si) is a high silicon MIG wire that improves wetting characteristics of the weld deposit. This alloy is used for joining of austenitic, manganese, work-hardenable steels, as well as armour plate and heat-resistant steels.

características

OK Autrod 16.95 is a continuous, solid, corrosion-resistant, chromium-nickel-manganese wire for welding austentic stainless alloys of the 18% Cr, 8% Ni, 7% Mn types. OK Autrod 16.95 has general corrosion resistance similar to that of the corresponding parent metal. When used for joining dissimilar materials, the corrosion resistance is of secondary importance.

OK Autrod 16.95
  • Welding Process
  • Soldadura con microalambre y gas de protección

clasificaciones

  • Classifications/Approvals

    • VdTUV
    • UDT

propiedades

Typical Properties
Yield Strength 65 ksi, 450 MPa
Tensile Strength 93 ksi, 640 MPa
Elongation in 2" 41 %
CVN at 20°F 96 ft-lbs, 130 J
Typical Undiluted Weld Metal Analysis  
C < 0.2 %
Mn 6.5 %
Si < 1.2 %
Cr 18.5 %
Ni 8.5 %

Part No.

OK Autrod 16.95
Part No. Model / Product Description UPC
169509982A ES OK 16.95 .9X15KG BAWS 662303079543
169511982A ES OK 16.95 1.2X15KG BAWS 662303081980
169510982A ES OK 16.95 040X33#BAWS 662303085865
169511932A ES OK 16.95 045X500#OMP 2/PLT 662303084608
169509932A ES OK 16.95 035X500#OMP 2/PLT 662303084615

SAW

Accessories

Depositions/Paramaters

Spray Transfer Deposition Table
Diameter Wire Feed Speed Amps Volts Deposition Rate
0.030 in, 0.8 mm 265-550 ipm, 673-1397 cm/min 160-210 24-28 6.5-9.6 lbs./hr., 2.95-4.35 kg./hr.
0.035 in, 0.9 mm 240-468 ipm, 610-1189 cm/min 170-255 24-30 7.8-12.7 lbs./hr., 2.54-5.76 kg./hr.
0.045 in, 1.2 mm 192-360 ipm, 488-914 cm/min 200-300 24-30 6.8-13.6 lbs./hr., 3.08-6.17 kg./hr.
1/16 in, 1.6 mm 120-192 ipm, 305-488 cm/min 215-325 24-32 7.3-14.5 lbs./hr., 3.31-6.58 kg./hr.
Shortarc Transfer Deposition Table
Diameter Wire Feed Speed Amps Volts Deposition Rate
0.03 in, 0.8 mm 156-312 ipm, 396-792 cm/min 40-120 15-20 1.4-3.8 lbs./hr., 0.64-1.72 kg./hr.
0.035 in, 0.9 mm 156-312 ipm, 396-792 cm/min 60-140 15-21 1.6-5.4 lbs./hr., 0.73-2.45 kg./hr.
0.045 in, 1.2 mm 140-280 ipm, 356-711 cm/min 100-210 17-22 2.4-6.0 lbs./hr., 1.09-2.72 kg./hr.
1.6 mm 550-900 ipm, 550-900 cm/min 230-375 23-31 11.5-19 lbs./hr., 5.2-8.6 kg./hr.