Los fundentes ESAB están diseñados para dar solución a una amplia variedad de requerimientos. Una línea completa de fundentes fundidos o aglomerados para las aplicaciones más comunes en el mercado.
Bonded fluxes are made by dry mixing the ingredients, then bonding them together with a low melting point compound. Most bonded fluxes contain metallic deoxidizers that prevent weld porosity, especially important in fillet welds. Fine ingredients are mechanically bonded into larger particles for good performance with one mesh size.
Fused fluxes are made by mixing the ingredients, then melting them together to form a chemically homogenous product. Because the ingredients are completely reacted in the manufacture, you get smooth stable performance and consistent weld metal properties.
Stainless submerged arc fluxes can be used with solid and metal cored wires. Regardless of the application, Alloy Rods have the right flux for joining or cladding of stainless and duplex steels.
All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.