All GTAW nickel based products are similarly produced (as are the ESAB stainless MIG wire), and meet a variety of demanding specifications. The chemically-cleaned wire surface prevents unnecessary impurities frequently associated with other TIG rods. All rods are marked with the proper identification to avoid lot mixups. The various grades and alloys make ESAB TIG products the first choice of welders.

Arcaloy ER276 (ERNiCrMo-4)
Arcaloy ER276 (ERNiCrMo-4)

Arcaloy ER276 es una aleación Ni-Cr-Mo diseñada para ensamblar o el revestimiento donde está esencial la resistencia a agrietarse de corrosión de tensión, a marcar con hoyos y a la corrosión de la grieta.

Arcaloy ER82 (ERNiCr-3)
Arcaloy ER82 (ERNiCr-3)

Arcaloy ER82 se utiliza para TIG, MIG, y VIO la soldadura de materias primas tales como aleaciones B163, B166, B167, y B168 de ASTM que tengan número N0660 de UNS.

Arcaloy ERNiCu-7
Arcaloy ERNiCu-7

Arcaloy ERNiCu-7, commonly referred to as Alloy FM60 is a GTAW (gas tungsten arc welding) product for welding nickel copper alloys such as ASTM B127, B163, B164 & B165, UNS number N04400.