Estas puntas de Swirljet están diseñadas para el uso con los sopletes manuales de fácil desconectado PREST-O-LITE® #1. Estos funcionan de manera silenciosa, se enfrían y dan una mejor transferencia de calor que cualquier punta que se compare.
| SKU | 21704 |
|---|---|
| UPC | 662067065127 |
| Model / Product Description | TIP AY SWIRLJET QD SJ 4A |
| Item Weight | 0.00 |
| Min Order | |
| Acetylene Swirljet Tips | |
| Fuel | Acetylene |
| Pressure | 13 PSIG |
| Gas Flow | 12.8 CFH |
| Copper Tubing Size And Capacity | |
| Soft Solder | 2-4 in |
| Silver Braze | 1-2 in |